| 000 | 03250nas|a2200421 i 4500 | ||
|---|---|---|---|
| 005 | 20260818090817.0 | ||
| 008 | 111099s1999 th uzm rtt 00| a1eng d | ||
| 035 | _a.b1176319x | ||
| 099 | 9 | _aAIT Thesis no. ST-99-10 | |
| 100 | 0 | _aDoan Thi Quynh Mai | |
| 245 | 1 | 0 | _aDevelopment of burnt bricks from waste sludge |
| 260 |
_aBangkok : _bAsian Institute of Technology, _c1999 |
||
| 300 |
_a72 leaves : _bill. |
||
| 490 | 1 |
_aThesis ; _vno. ST-99-10 |
|
| 502 | _aThesis (M.Eng.) - Asian Institute of Technology, 1999 | ||
| 500 | _aA thesis submitted in partial fulfillment of the requirements for the degree of Master Engineering, School of Civil Engineering | ||
| 520 | _aRapid urbanization in countries all over the world has resulted in a drastic increase of waste sludge. Sludge resulting from wastewater treatment plants creates problems of disposal. There are many solutions of disposal applied such as spreading on the land, landfilling or incineration. However, the future trends in sludge management are towards reutilization as useful resource. This study presents the results of the utilization waste sludge as brickmaking material in small-scale brickmaking condition. Two types of sludge used in research work are organic and inorganic for comparison. Bricks with a range of sludge and pozzolan combined from rice husk ash and fly ash are prepared manually and then fired in a small-scale brick factory. Measurements of shrinkage, water absorption capacity and compressive strength of bricks are conducted. Test results indicated that the utilization of sludge as clay-replacing material in small-scale brickmaking in developing countries is feasible. The quality of bricks made from inorganic sludge is better than that of bricks made from organic sludge. Compressive strength of bricks using inorganic sludge is satisfactory, comparing to ordinary bricks manufactured in the same condition. Due to high shrinkage and lower compressive strength, bricks using organic sludge are not attractive | ||
| 650 | 0 | _aSewage sludge | |
| 650 | 0 | _aBrickmaking | |
| 700 | 0 |
_aPichai Nimityongskul, _eChairperson |
|
| 700 | 1 |
_aGupta, Satyendra P., _eExamination committee |
|
| 700 | 1 |
_aKishi, Toshiharu, _eExamination committee |
|
| 710 | 2 |
_aAsian Development Bank (ADB),Japan, _eScholarship donor |
|
| 810 | 2 |
_aAsian Institute of Technology. _tThesis ; _vno. ST-99-10 |
|
| 856 |
_3Full-Text _uhttp://203.159.5.9/ait-thesis/detail.php?q=B12699 |
||
| 907 |
_a.b1176319x _bmnait _cy |
||
| 902 | _a240419 | ||
| 998 |
_b0 _c991011 _dm _ea _fy _g0 |
||
| 945 | _lmnait | ||
| 945 | _lmnait | ||
| 945 | _lmnarc | ||
| 942 | _c20 | ||
| 942 | _c40 | ||
| 909 |
_aBarcode : 30050120709091 _bCREATED : 1998-05-14 _cRECORD # : i12155251 _dLPATRON : 1017964 _eLCHKIN : 2005-02-27 _f# RENEWALS : 0 _g# OVERDUE : 0 _hIUSE3 : 0 _iTOT CHKOUT : 5 _jTOT RENEW : 2 |
||
| 909 |
_aBarcode : 30050120709067 _bCREATED : 1998-05-14 _cRECORD # : i12155263 _dLPATRON : 1011384 _eLCHKIN : 2000-01-19 _f# RENEWALS : 0 _g# OVERDUE : 0 _hIUSE3 : 0 _iTOT CHKOUT : 2 _jTOT RENEW : 0 |
||
| 909 |
_aBarcode : 30050160101688 _bCREATED : 2016-04-21 _cRECORD # : i12944919 _dLPATRON : 0 _eLCHKIN : - _f# RENEWALS : 0 _g# OVERDUE : 0 _hIUSE3 : 0 _iTOT CHKOUT : 0 _jTOT RENEW : 0 |
||
| 999 |
_c29208 _d29208 |
||